What 300-mm SiC Brings to AI Chip Packaging
Original source (powerelectronics)
Share Article:

SiC suppliers, including Coherent and Wolfspeed, are moving to 300 mm to bring the material into advanced AI packaging. Coherent has started sampling its 300-mm, high-thermal-conductivity SiC substrates to AI semiconductor partners, extending its SiC materials platform into heat spreaders and related packaging applications. The news follows the company’s earlier development of 200-mm SiC substrates.

SiC already offers high thermal conductivity, mechanical strength, and thermal stability at smaller wafer sizes. But moving to a larger wafer of 300 mm does not inherently make the material conduct heat better. The larger format aligns SiC with the wafer size used across memory and much of the equipment supporting wafer-level advanced packaging.

Both Coherent and Wolfspeed are trying to introduce a high-thermal-conductivity material into a manufacturing ecosystem built around 300-mm wafers. This requires control over crystal growth, wafer geometry, and surface preparation, followed by package integration that maintains the thermal advantage of bulk SiC.

Why wafer size matters for SiC in AI packaging

Advanced AI processors have large compute dies or chiplets with high-bandwidth memory and other components. As these grow, their heat sources become distributed unevenly across a larger footprint. But localized regions produce hotspots even when the package has access to a cold plate or liquid-cooling system.

In such environments, SiC’s high thermal conductivity spreads concentrated heat laterally, while the 300-mm format lets it be processed with existing packaging tools.

The 300-mm diameter provides semiconductor manufacturers with a material form that aligns with existing carriers, wafer-handling systems, bonding platforms, and metrology used in advanced semiconductor manufacturing.

This also changes how the material can be processed. Instead of treating SiC only as an individual package component, manufacturers can perform cleaning, deposition, metallization, bonding, thinning, inspection, and singulation using wafer-level process flows. Coherent describes its substrates as compatible with existing semiconductor manufacturing platforms.

In practice, compatibility requires the substrate to operate efficiently with 300-mm carriers and robotic handling, provide acceptable edge geometry and wafer shape, and establish stable contact with bonding tools.

The importance of 300 mm comes from combining SiC’s thermal properties with the manufacturing infrastructure already serving advanced logic and packaging.

Making SiC fit the 300-mm packaging ecosystem

Reaching the required standard starts with the SiC crystal itself. Coherent, for example, uses physical vapor transport (PVT) for bulk SiC growth, and increasing the diameter from 200 to 300 mm expands the wafer area by 2.25×. The furnace must control the growth interface over a much larger area without creating excessive differences between the center and edge.

During growth, the temperature difference between the source and seed helps move SiC vapor toward the growing crystal (Figure 1). Temperature differences across the wafer also affect the shape of the growth front and the stress inside the crystal. If the growth front becomes too curved, stacking faults and other defects can form.

Uneven temperatures can also leave stress in the crystal and increase the risk of dislocations. Coherent’s large-diameter PVT patents describe changes to the heater, crucible, and insulation that help create a flatter growth front and direct more heat along the growth direction.

PVT SiC crystal growth.
Figure 1: PVT SiC crystal growth (Source: Wikimedia Commons)

From there, the boule must become a wafer that semiconductor packaging equipment can handle. Coherent says its SiC operation is vertically integrated across crystal growth, wafering, polishing, and characterization. This is useful because stresses introduced during growth can affect the finished wafer after slicing and polishing.

The larger diameter also increases the difficulty of controlling slicing damage, thickness variation, and edge quality. Grinding and chemical mechanical polishing must remove damaged material and produce the required surface without introducing additional nonuniformity.

For packaging, these operations determine bow, warp, total thickness variation, and surface condition. Those parameters affect wafer handling, chuck contact, and bonding. The real value of Coherent’s sampling is that the company has progressed far enough to supply finished substrates for customers to evaluate inside semiconductor manufacturing.

Wolfspeed is pursuing the same packaging opportunity. Building on its January 2026 production of a single-crystal 300-mm SiC wafer, the company is working with foundries, OSATs, and research institutions to evaluate SiC interposers and heat spreaders for large AI and HPC packages (Figure 2).

AI package showing a SiC interposer beneath the compute and high-bandwidth-memory layer.
Figure 2: AI package showing a SiC interposer beneath the compute and high-bandwidth-memory layer (Source: Wolfspeed)

What 300-mm SiC does inside an AI package

Once SiC enters the package, its thermal conductivity takes on a more complex role.

Coherent says its 300-mm substrates are engineered to provide up to 25% more heat spreading than current solutions. The physical basis for that benefit starts with the nonuniform way that AI processors generate heat.

Heat leaving a small hotspot does not only move vertically toward the cooling system; it spreads laterally as it enters a larger layer above the die. Higher thermal conductivity reduces this spreading resistance and allows more of the cold-side area to help in heat removal.

Once the substrate is bonded into the package, heat must cross interfaces between the die, bonding material, SiC, and cooling structure. Voids, oxides, adhesives, solder layers, or other interface materials introduce additional thermal resistance.

Direct or hybrid bonding can reduce bond-line thickness, but these processes place tighter requirements on flatness, cleanliness, and surface preparation.

SiC’s thermal expansion is much closer to silicon’s than copper’s is, which helps with package integration, but its high stiffness means stress must still be managed across a heterogeneous stack during temperature cycling.

The 25% claim is best understood as a heat-spreading target at the package level. The final efficiency will depend on how effectively the package converts the bulk thermal conductivity into a lower-resistance path for heat to flow from localized AI hotspots to the cooling system.

The significance of 300-mm SiC lies in bringing a high-thermal-conductivity material into the same manufacturing format already used for leading-edge AI processors and advanced packaging.

If suppliers can translate SiC’s bulk thermal properties into repeatable wafer-level processing and package-level heat spreading, 300-mm SiC could establish a new role for SiC as a thermal management material.

Major player builds functional power devices on 300-mm SiC

Beyond using SiC for heat spreading and interposers, Infineon recently announced its own 300-mm SiC milestone, this time with functional power devices. Speaking with Power Electronics News at electronica 2026, Adam White, division president of Power Systems at Infineon, called it “the incredible world first: 300 mm SiC with functional, working devices.” The wafers were processed at the company’s Villach, Austria, fab using existing silicon manufacturing equipment.

Cover image: Adobe Stock

Tags: AI, Chips, SiC, Silicon Carbide

Source: Power Electronics News